Compare

Chemistry

Acrylic

Epoxy

Materials

Composite Resins

Composite Resins

Processes

Composite stratification

Composite stratification

Application

Rigid socket by lamination

Rigid socket by lamination

Rigid socket by lamination

Ratio

100 : 2~3

100 / 40

Resin viscosity

250 mPa.s

Temps au pic d’exothermie

25 min

Demoulding time at 20°C

35 min

Hardness

85 Shore D

85 Shore D

Gamme

COPACRYL

ORTHOPOXY

Références

CAC F01, CAC F05, CAC F25

Accessories

Composite Reinforcements

Composite Reinforcements

Orhopedic

Type of fiber

Natural

Natural

Reinforcement composition

Flax fibers

Length

5 m

50mL

Grammage/Diamètre

130 g/mL – 130 mm, 203 g/mL – 150 mm

Tailles

T12 à T6

Number of units per batch

20

Mix viscosity at 20°C

450 mPa.s

Working time at 20°C

30min

Temps de gel en couche mince à 20°C

1 h 30

Post curing

1 h à 100 °C

Bio based

45 %