Epoxy |
Composite Resins |
Rigid socket by lamination |
Composite stratification |
100 / 40 |
450 mPa.s |
30 min |
1 h 30 |
1 hat 100 °C |
85 Shore D |
45 % |
ORTHOPOXY |
Epoxy |
Composite Resins |
Rigid socket by lamination |
Composite stratification |
100 / 40 |
450 mPa.s |
30 min |
1 h 30 |
1 hat 100 °C |
85 Shore D |
45 % |
ORTHOPOXY |